Comparison of the corrosion and stress-corrosion behavior of a ternary Al-Zn-Mg alloy

  • PDF / 507,390 Bytes
  • 5 Pages / 612 x 792 pts (letter) Page_size
  • 53 Downloads / 380 Views

DOWNLOAD

REPORT


Comparison of the Corrosion and Stress-Corrosion Behavior of a Ternary AI-Zn-Mg Alloy A. J. SEDRIKS, J. A. S. GREEN, AND D. L. NOVAK A c o m p a r i s o n has b e e n made of the c o r r o s i o n and s t r e s s - c o r r o s i o n b e h a v i o r of an aged A1-5.3 wt pct Z n - 2 . 5 wt pet Mg alloy in aqueous c h l o r i d e solutions of v a r y i n g pH (i.e., 1 to 6.2). It is found that l o w e r i n g the pH to v a l u e s