Page 1518: In Figure 17 the unlabeled composite showing a 300 pct increase in creep strength at 700 K is #6005.

Correction to Metall. Trans. A, 1983, vol. 14A The Kinetics of ~r-Phase Precipitation in AISI 310 and AISI 316 Steels by Jan Barcik Page 636: Table III: The Isolate Phase Composition for Electrolyte Number I should read "carbides and o-phase" (not "carbides and a-phase", as printed).

406--VOLUME 15A, FEBRUARY 1984