Constant amplitude fatigue crack growth rate tests were conducted on a nickel base superalloy IN718 at various stress ratios, R ranging from R = 0.1 to 0.7. Tests were conducted at room temperature and in lab air atmosphere. Tests were performed in a 100 

  • PDF / 39,987,360 Bytes
  • 645 Pages / 439.37 x 666.142 pts Page_size
  • 9 Downloads / 406 Views

DOWNLOAD

REPORT


S. Seetharamu Thimmarayappa Jagadish Ravindra R. Malagi Editors

Fatigue, Durability, and Fracture Mechanics Proceedings of Fatigue Durability India 2019

Lecture Notes in Mechanical Engineering Series Editors Francisco Cavas-Martínez, Departamento de Estructuras, Universidad Politécnica de Cartagena, Cartagena, Murcia, Spain Fakher Chaari, National School of Engineers, University of Sfax, Sfax, Tunisia Francesco Gherardini, Dipartimento di Ingegneria, Università di Modena e Reggio Emilia, Modena, Italy Mohamed Haddar, National School of Engineers of Sfax (ENIS), Sfax, Tunisia Vitalii Ivanov, Department of Manufacturing Engineering Machine and Tools, Sumy State University, Sumy, Ukraine Young W. Kwon, Department of Manufacturing Engineering and Aerospace Engineering, Graduate School of Engineering and Applied Science, Monterey, CA, USA Justyna Trojanowska, Poznan University of Technology, Poznan, Poland

Lecture Notes in Mechanical Engineering (LNME) publishes the latest developments in Mechanical Engineering—quickly, informally and with high quality. Original research reported in proceedings and post-proceedings represents the core of LNME. Volumes published in LNME embrace all aspects, subfields and new challenges of mechanical engineering. Topics in the series include: • • • • • • • • • • • • • • • • •

Engineering Design Machinery and Machine Elements Mechanical Structures and Stress Analysis Automotive Engineering Engine Technology Aerospace Technology and Astronautics Nanotechnology and Microengineering Control, Robotics, Mechatronics MEMS Theoretical and Applied Mechanics Dynamical Systems, Control Fluid Mechanics Engineering Thermodynamics, Heat and Mass Transfer Manufacturing Precision Engineering, Instrumentation, Measurement Materials Engineering Tribology and Surface Technology

To submit a proposal or request further information, please contact the Springer Editor of your location: China: Dr. Mengchu Huang at [email protected] India: Priya Vyas at [email protected] Rest of Asia, Australia, New Zealand: Swati Meherishi at [email protected] All other countries: Dr. Leontina Di Cecco at [email protected] To submit a proposal for a monograph, please check our Springer Tracts in Mechanical Engineering at http://www.springer.com/series/11693 or contact [email protected] Indexed by SCOPUS. The books of the series are submitted for indexing to Web of Science.

More information about this series at http://www.springer.com/series/11236

S. Seetharamu Thimmarayappa Jagadish Ravindra R. Malagi •



Editors

Fatigue, Durability, and Fracture Mechanics Proceedings of Fatigue Durability India 2019

123

Editors S. Seetharamu Central Power Research Institute Bangalore, Karnataka, India

Thimmarayappa Jagadish DHIO Research and Engineering Pvt Ltd Bangalore, Karnataka, India

Ravindra R. Malagi Mechanical Department KLS Gogte Institute of Technology Belagavi, Karnataka, India

ISSN 2195-4356 ISSN 2195-4364 (electronic) Lecture Notes in Mechanical Engineering ISBN 97