Effect of Heat Treatment on Microstructure and Mechanical Properties of ODS Nickel-Based Superalloy via Strengthening Me

  • PDF / 2,259,578 Bytes
  • 9 Pages / 593.972 x 792 pts Page_size
  • 90 Downloads / 310 Views

DOWNLOAD

REPORT


https://doi.org/10.1007/s11837-020-04220-6 Ó 2020 The Minerals, Metals & Materials Society

TECHNICAL ARTICLE

Effect of Heat Treatment on Microstructure and Mechanical Properties of ODS Nickel-Based Superalloy via Strengthening Mechanism GUOWEI WANG ,1,2,3 LAN HUANG,1,2,3 PENGYANG ZHAO,4 XIN ZHAN,1,2,3 ZIJUN QIN,1,2,3 WUQIANG HE,1,2,3 FENG LIU,1,2,3,6 and YAN NIE5 1.—State Key Laboratory of Powder Metallurgy, Central South University, Changsha 410083, China. 2.—Powder Metallurgy Research Institute, Central South University, Changsha 410083, China. 3.—High Temperature Materials Research Institute, Central South University, Changsha 410083, China. 4.—Department of Engineering Mechanics, Shanghai Jiao Tong University, 800 Dongchuan Road, Shanghai 200240, China. 5.—Yuanmeng Precision Technology (Shenzhen) Institute, Shenzhen, China. 6.—e-mail: [email protected]

The microstructure and mechanical properties of oxide-dispersion-strengthened nickel-based superalloy (ODSN) are related to its thermal stability and pose an essential challenge in modeling. This study focuses on the relationship between the microstructure and yield strength of heat-treated ODSN. Through a comprehensive description of the microstructure as investigated by electron-backscatter diffraction analysis and transmission electron microscopy, the contributions to the yield strength arising from various strengthening mechanisms in heat-treated ODSN specimens are addressed. The yield strength calculated using the characterized microstructure parameters in combination with different strengthening models are compared with the measured yield strength. This comparison reveals that grain-boundary strengthening, followed by dispersion and dislocation strengthening, is the significant contributor, while a root-sum-square superposition model reproduces the measured yield strength of heat-treated ODSN within the experimental scatter.

INTRODUCTION Compared with other, conventional alloys, oxidedispersion-strengthened (ODS) alloys exhibit remarkable tensile strength and creep strength, as well as good radiation damage tolerance because of the presence of uniformly dispersed nanooxide particles. Previous studies on ODS iron-based alloys have clearly shown that nanoparticles act as barriers to dislocation motion and grain-boundary migration, controlling the high-temperature tensile properties and creep resistance.1 Moreover, nanoparticles provide effective absorption of radiation-induced defects, such as vacancies and interstitials, as well as nucleation sites for helium to inhibit bubble formation and ultimately provide high radiation resistance.2,3 However, long-term service of ODS iron-based alloys is only possible at

temperatures of 700°C or less; by contrast, ODS nickel-based superalloy (ODSN) exhibits excellent creep, fatigue, and oxidation resistance at temperatures greater than 1000°C.4 Therefore, ODSN is considered to be an attractive candidate for use in high-temperature environments such as those encountered in aerospace.5,6 and nuclear industry applica