Role of Ru on the Microstructural Evolution During Long‑Term Aging of Ni‑Based Single Crystal Superalloys Wei Song1 · Xin‑Guang Wang1 · Jin‑Guo Li1 · Ye‑Shun Huang1 · Jie Meng1 · Yan‑Hong Yang1 · Jin‑Lai Liu1 · Ji‑De Liu1 · Yi‑Zhou Zhou1 · Xiao‑Feng Sun1 Received: 8 April 2020 / Revised: 20 May 2020 / Accepted: 21 May 2020 © The Chinese Society for Metals (CSM) and Springer-Verlag GmbH Germany, part of Springer Nature 2020
Abstract Two experimental alloys containing different contents of Ru were investigated to study the effect of Ru on the microstructural evolution during long-term thermal exposure. The increase in Ru promoted the formation of cubical, tiny, and even γ′ phase after full heat treatment. Moreover, the samples after full heat treatment were exposed at 1100 °C for different time. Based on the classical model by Lifshitz, Slyozov, and Wagner, the coarsening of γ′ phase of the alloy containing 2.5 and 3.5 wt.% Ru during the long-term aging was controlled by the interface reaction and diffusion, respectively. The γ/γ′ lattice misfit was more negative with the increment of Ru addition, which induced the formation of stable rafted γ′ phase in the alloy containing 3.5 wt.% Ru at the initiation of long-term aging. Besides, the increase in Ru reduced the diffusion coefficient, which could restrain the γ′ phase coarsening. The lower γ/γ′ lattice misfit of the alloy containing 2.5 wt.% Ru promoted the interface reaction, which induced the rapid coarsening of γ′ phase. Therefore, the increase in Ru improved the microstructural stability of the alloys. On the other hand, the raise of Ru induced “reverse partitioning” behavior, which was effective in suppressing the emergence of the topologically close-packed phase (TCP phase). The TCP phase occasionally occurred in the alloy containing 2.5 wt.% Ru, which was attributed to the high temperature and the supersaturation of the γ matrix. Moreover, the TCP phase was determined as μ phase, which had a high concentration of Co, Re, Mo, and W. A sketch map describing the evolution of the TCP phase was also constructed. Keywords Ni-based superalloys · Ruthenium · Coarsening · TCP phase
1 Introduction Nickel-based single crystal superalloys have been the outstanding candidate materials for aerospace, gas turbine, and energy chemical industry due to its prominent creep and oxidation resistance at elevated temperatures [1–4]. In pace with the continuous increase in the turbine inlet temperatures [5], the service temperatures of superalloys need Available online at http://link.springer.com/journal/40195. * Xin‑Guang Wang [email protected] * Jin‑Guo Li [email protected] * Xiao‑Feng Sun [email protected] 1
Superalloys Division, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
further improvement. Therefore, in recent years, a considerable quantity of refractory elements such as Re, W, and Mo is added to superalloys to enhance the solution strengthening effects and oxidation resistance properties, which can significantly improve the service