Solving Recent Challenges for Wrought Ni-Base Superalloys

  • PDF / 2,364,013 Bytes
  • 25 Pages / 593.972 x 792 pts Page_size
  • 19 Downloads / 235 Views

DOWNLOAD

REPORT


Solving Recent Challenges for Wrought Ni-Base Superalloys M.C. HARDY, M. DETROIS, E.T. MCDEVITT, C. ARGYRAKIS, V. SARAF, P.D. JABLONSKI, J.A. HAWK, R.C. BUCKINGHAM, H.S. KITAGUCHI, and S. TIN This paper reviews the status of technology in design and manufacture of new wrought polycrystalline Ni-base superalloys for critical engineering applications. There is a strong motivation to develop new alloys that are capable of operating at higher temperatures to realize improvements in thermal efficiency, which are necessary to achieve environmental targets for reduced emissions of harmful green-house gases. From the aerospace sector, the development of new powder metallurgy and ingot metallurgy alloys is discussed for disk rotor and static applications. New compositions for powder metallurgy contain about 50 to 55 pct of gamma prime (c¢) strengthening precipitates to ensure components operate successfully at temperatures up to 788 C (1450 F). In contrast, new compositions for ingot metallurgy aim to occupy a design space in temperature capability between Alloy 718 and current powder alloys that are in-service, and show levels of c¢ of about 30 to 44 pct. The focus in developing these alloys was design for manufacturability. To complement the aerospace developments, a review of work to understand the suitability of candidate alloys for multiple applications in Advanced-Ultra Supercritical (AUSC) power plants has been undertaken by Detrois, Jablonski, and Hawk from the National Energy Technology Laboratory. In these power plants, steam temperatures are required to reach 700 C to 760 C. The common thread is to develop alloys that demonstrate a combination of high-temperature properties, which are reliant on both the alloy composition and microstructure and can be produced readily at the right price. For the AUSC applications, the emphasis is on high-temperature strength, long-term creep life, phase stability, oxidation resistance, and robust welding for fabrications. Whereas for powder disk rotors in aircraft engines, the priority is enhanced resistance to time-dependent crack growth, phase stability, and resistance to environmental damage, while extending the current strength levels, which are shown by existing alloys, to higher temperatures. https://doi.org/10.1007/s11661-020-05773-6  The Minerals, Metals & Materials Society and ASM International 2020

M.C. HARDY, C. ARGYRAKIS and R. C. BUCKINGHAM are with the Rolls-Royce plc, PO Box 31, Derby, DE24 8BJ, UK. Contact e-mail: [email protected]. M. DETROIS is with the U.S. Department of Energy, National Energy Technology Laboratory, 1450 Queen Ave., SW, Albany, OR 97321, USA and LRST, 1450 Queen Ave. SW, Albany, OR 97321, USA. E. T. MCDEVITT is with the Allegheny Technologies Incorporated Specialty Materials, 2020 Ashcraft Avenue, PO Box 5030, Monroe, NC 28111, USA. V. SARAF is with the Allegheny Technologies Incorporated Forged Products Cudahy, PO Box 8902, 5481 S. Packard Avenue, Cudahy, WI 53110, USA. P. D. JABLONSKI and J. A. HAWK are with the U.S. Department