Surface Acoustic Wave Characterization of Pitting Corrosion Damage with Fatigue Cracks
The design goals for length of operation of the present aircraft generation will be exceeded by most operators of jet-powered airplanes and turboprops [1]. The design was performed for fatigue life related to total flight hours or total number of cycles d
- PDF / 43,931,265 Bytes
- 435 Pages / 439.37 x 666.142 pts Page_size
- 103 Downloads / 289 Views
MATERIALS SCIENCE
Physics and Astronomy springeronline.com
Springer-Verlag Berlin Heidelberg GmbH
ONLINE L1BRARY
Springer Series in
MATERIALS SCIENCE Editors: R. Hull
R. M. Osgood, Jr.
J. Parisi
H. Warlimont
The Springer Series in Materials Science covers the complete spectrum of materials physics, including fundamental principles, physical properties, materials theory and design. Recognizing the increasing importance of materials science in future device technologies, the book titles in this series reflect the state-of-the-art in understanding and controlling the structure and properties of all important classes of materials. 61 Fatigue in Ferroelectric Ceramics and Related Issues By D.C. Lupascu
66 Multiphased Ceramic Materials Processing and Potential Editors: W.-H. Tuan and J.-K. Guo
62 Epitaxy Physical Foundation and Technical Implementation By M.A. Herman, W. Richter, and H. Sitter
67 Nondestructive Materials Characterization With Applications to Aerospace Materials Editors: N.G.H. Meyendorf, P.B. Nagy, and S.1. Rokhlin
63 Fundamentals ofIon Irradiation ofPolymers ByD. Fink 64 Morphology Control of Materials and Nanoparticles Advanced Materials Processing and Characterization Editors: Y. Waseda and A. Muramatsu 65 Transport Processes in Ion Irradiated Polymers ByD. Fink
68 Diffraction Analysis of the Microstructure of Materials Editors: E.J. Mittemeijer and P. Scardi 69 Chemical-Mechanical Planarization of Semiconductor Materials Editor: M.R. Oliver 70 Isotope Effect Applications in Solids By G.V. Plekhanov
Series homepage - http://www.springer.de/physlbooks/ssms/ Volumes lO-60 are listed at the end of the book.
Norbert G.H. Meyendorf Peter B. Nagy Stanislav I. Rokhlin (Eds.)
Nondestructive Materials Characterization With Applications to Aerospace Materials
With 311 Figures and 11 Tables
"
Springer
Professor Norbert G.H. Meyendorf University of Dayton Center for Materials Diagnostics 300 College Park Dayton, OH 45469-0121, USA E-mail: [email protected]
Professor Peter B. Nagy University of Cincinnati Dept. of Aerospace Engineering and Engineering Mechanics MLo070, Cincinnati, OH 45221, USA E-mail: [email protected]
Professor Stanislav I. Rokhlin The Ohio State University Dept. of Industrial, Welding and Systems Engineering 1248 Arthur E. Adams Drive Columbus, OH 43221, USA E-mail: [email protected]
Series Editors: Professor Robert Hull
Professor Jürgen Parisi
University of Virginia Dept. of Materials Science and Engineering Thornton Hall Charlottesville, VA 22903-2442, USA
Universität Oldenburg, Fachbereich Physik Abt. Energie- und Halbleiterforschung Carl-von-Ossietzky-Strasse 9-11 26129 Oldenburg, Germany
Professor R. M. Osgood, Jr.
Professor Hans Warlimont
Microelectronics Science Laboratory Department of Electrical Engineering Columbia University Seeley W. Mudd Building New York, NY 10027, USA
Institut für Festkörperund Werkstofforschung, Heimholtzstrasse 20 01069 Dresden, Germany
ISSN 0933-033X ISBN 978-3-642-07350-2 ISBN 978-3-662-08988-0 (eBook) DOI 10.1007/9