IN the original article the captions for Figures 7, 8, and 9 were correct, but the images were incorrect. Following are the correct images with their captions:

YUAN TIAN, Ph.D. Student, RAYNALD GAUVIN, Professor, and MATHIEU BROCHU, Associate Professor, are with the Department of Mining and Materials Engineering, McGill University, Montreal, QC H3A 0C5, Canada. Contact e-mail: mathieu.brochu@ mcgill.ca The online version of the original article can be found under doi:10.1007/s11661-016-3505-8. Article published online May 18, 2016 3782—VOLUME 47A, JULY 2016

METALLURGICAL AND MATERIALS TRANSACTIONS A

Fig. 7—Measurement of dendrite tip radius in top clads: (a) low magnification dendritic structure; (b) estimation of dendrite tip radius (15 nm); (c) low magnification dendritic structure; and (d) estimation of dendrite tip radius (30 nm).

Fig. 8—KGT model describing the dendrite tip radius as a function of SFV.

METALLURGICAL AND MATERIALS TRANSACTIONS A

Fig. 9—Effective partition coefficient of B as a function of SFV.