Structural and Fractographic Features of Gas Pipeline Steel Degradation

Structural and fractographic features of degradation are analyzed for pipe steels after their operation on main gas pipelines. The structural feature of steel degradation is damaging along the boundaries between pearlite and ferrite grains manifested by m

  • PDF / 11,529,160 Bytes
  • 248 Pages / 453.543 x 683.15 pts Page_size
  • 97 Downloads / 342 Views

DOWNLOAD

REPORT


Gabriella Bolzon Giovanna Gabetta Hryhoriy Nykyforchyn   Editors

Degradation Assessment and Failure Prevention of Pipeline Systems

Lecture Notes in Civil Engineering Volume 102

Series Editors Marco di Prisco, Politecnico di Milano, Milano, Italy Sheng-Hong Chen, School of Water Resources and Hydropower Engineering, Wuhan University, Wuhan, China Ioannis Vayas, Institute of Steel Structures, National Technical University of Athens, Athens, Greece Sanjay Kumar Shukla, School of Engineering, Edith Cowan University, Joondalup, WA, Australia Anuj Sharma, Iowa State University, Ames, IA, USA Nagesh Kumar, Department of Civil Engineering, Indian Institute of Science Bangalore, Bengaluru, Karnataka, India Chien Ming Wang, School of Civil Engineering, The University of Queensland, Brisbane, QLD, Australia

Lecture Notes in Civil Engineering (LNCE) publishes the latest developments in Civil Engineering - quickly, informally and in top quality. Though original research reported in proceedings and post-proceedings represents the core of LNCE, edited volumes of exceptionally high quality and interest may also be considered for publication. Volumes published in LNCE embrace all aspects and subfields of, as well as new challenges in, Civil Engineering. Topics in the series include: • • • • • • • • • • • • • • •

Construction and Structural Mechanics Building Materials Concrete, Steel and Timber Structures Geotechnical Engineering Earthquake Engineering Coastal Engineering Ocean and Offshore Engineering; Ships and Floating Structures Hydraulics, Hydrology and Water Resources Engineering Environmental Engineering and Sustainability Structural Health and Monitoring Surveying and Geographical Information Systems Indoor Environments Transportation and Traffic Risk Analysis Safety and Security

To submit a proposal or request further information, please contact the appropriate Springer Editor: – Mr. Pierpaolo Riva at [email protected] (Europe and Americas); – Ms. Swati Meherishi at [email protected] (Asia - except China, and Australia, New Zealand); – Dr. Mengchu Huang at [email protected] (China). All books in the series now indexed by Scopus and EI Compendex database!

More information about this series at http://www.springer.com/series/15087

Gabriella Bolzon Giovanna Gabetta Hryhoriy Nykyforchyn •



Editors

Degradation Assessment and Failure Prevention of Pipeline Systems

123

Editors Gabriella Bolzon Dipartimento di Ingegneria Civile e Ambientale Politecnico di Milano Milano, Italy

Giovanna Gabetta Oil&Gas Sector Milano, Italy

Hryhoriy Nykyforchyn Karpenko Physico-Mechanical Institute National Academy of Sciences of Ukraine Lviv, Ukraine

ISSN 2366-2557 ISSN 2366-2565 (electronic) Lecture Notes in Civil Engineering ISBN 978-3-030-58072-8 ISBN 978-3-030-58073-5 (eBook) https://doi.org/10.1007/978-3-030-58073-5 © The Editor(s) (if applicable) and The Author(s), under exclusive license to Springer Nature Switzerland AG 2021 This work is subject to copyright. All rights are solely and exclusive